A supplier’s comparison sheet has one box headed “bending strength”. The source document for the specified slate gives two values with the same units. Entering the larger number or taking their average would remove information the reviewer needs to evaluate the proposed substitute.
For example, Welsh Slate’s January 2025 document for Cwt-y-Bugail Capital grade lists a characteristic modulus of rupture of 66.6 N/mm² in the transverse direction and 28.7 N/mm² in the longitudinal direction. Both entries belong to the same named product. The manufacturer’s explanation uses the two directions separately in relating strength and slate dimensions to thickness.
Give each direction its own column
Label two cells with the full direction names and units before entering either value. Keep the document reference, grade, date and test method in the same row. If an alternative supplier lists a single figure, ask which direction it represents and whether it is a characteristic value calculated on the same basis. Leave the other direction open until the supplier supplies supporting data. Repeating the one number across both columns makes a partial report appear complete.
When the slate dimensions change as well as the stone, flag the size change for the designer. These material test results do not give an allowable load on a finished roof. The Guild’s guide to force and stress units explains an additional check when another sheet reports its test results in pounds.