A reviewer highlights 283 on a clay tile test sheet and writes “below 300.” The number is in the right row, but which requirement goes with it? The American Test Lab of South Florida’s published report for Verea Flat tiles gives a worked example.
On page two, the row for dry transverse breaking strength has five specimen results in pounds-force. The lowest is 283. The report gives 250 as the minimum for any one specimen and 300 as the minimum for the five-piece average. The laboratory reports an average of 305. By the comparisons printed on that row, both requirements are met. Comparing each tile to 300 would incorrectly flag two specimens.
Preserve the qualifiers on the review sheet
Enter the model, test condition, lowest individual result and average in separate fields. Label the unit “pounds-force.” These values describe how the specimens broke in the laboratory. They cannot supply a permissible foot-traffic load on an installed roof.
Read the signed conclusion before releasing the submittal. In this report the laboratory calls out exceptions involving average height and individual thickness. A reviewer could record the strength row as meeting its printed limits and still flag dimensions for resolution. Attach the complete report to the clay tile submittal so the next reader can see both decisions. For a current project, obtain evidence for the tile actually offered and the edition named in the project documents.